The Hardening Processes of The Ball and Seat of Metal Hard Seal Ball Valves


Release time:

Aug 25,2024

The Hardening Processes of The Ball and Seat of Metal Hard Seal Ball Valves

     Metal hard seal ball valve ball and seat with reasonable hardening process, can improve the service life and performance of the direct decision metal hard seal valve, reasonable hardening process can reduce manufacturing costs. At present, the following hardening ways are commonly used on the surface of metal hard seal ball valves:

                                                            

     (1) Surfacing (or spray welding) cemented carbide on the surface of the ball. Hardness up to 40HRC or more, the ball surface surfacing carbide process is complex, low production efficiency, and a large area of surfacing easy to make the parts deformation, the current hardening of the ball surface of the process to use less.

    (2) Ball surface hard chrome plating, hardness up to 60-65HRC, thickness 0.07 ~ 0.10ram, chrome layer hardness, wear-resistant, corrosion-resistant and can keep the surface bright for a long time, the process is relatively simple, the cost is low. However, the hardness of hard chrome plating in the temperature rise will be due to the release of internal stress and rapid reduction of its working temperature cannot be higher than 427 ℃. In addition, the bonding force of the chromium plating layer is low, and the plating layer is easy to fall off.

     (3) The surface of the ball using plasma nitriding, surface hardness up to 60 ~ 65HRC, nitriding layer thickness of 0.20-0.40mm, plasma nitriding treatment hardening process due to poor corrosion resistance, cannot be used in the chemical industry and other areas of strong corrosion.

     (4) Ball surface supersonic spraying (HVOF) process, the hardness of up to 70 ~ 75HRC, collection of high strength, thickness of 0.3-0.4mm, supersonic spraying is the main means of surface hardening of the sphere process. Supersonic spraying process is a process in which the combustion of oxygen fuel produces a high-speed airflow to accelerate the impact of powder particles on the surface of the workpiece to form a dense surface coating. During the impact process, due to the high speed of the particles (500-750m/s) and the low temperature of the particles (-3000℃), a coating with high bonding strength, low void ratio and low oxide content can be obtained after the impact on the surface of the workpiece.

     Spray welding and cladding hardening process in the cemented carbide and the substrate have a melting process, the cemented carbide and the substrate collection at the hot melt zone, in order to fully achieve the performance of the spray welding or cladding of cemented carbide layer, to avoid the processing of welding after the weld hot melt zone for the metal contact surface, the thickness of the spray welding or cladding of cemented carbide thickness needs to be greater than 3mm or more.